DECAY RESISTANCE, PHYSICAL, MECHANICAL, AND THERMAL PROPERTIES OF HEATED ORIENTAL BEECH WOOD
(Slovak Forest Products Research Inst, 2015)
Heat treatment of Oriental beech (Fagus orientalis) wood was carried out by hot air in an oven for 2, 6, and 10 h at 125, 155, and 185 degrees C. After heat treatment; decay resistance, oven dry density, modulus of rupture ...
SURFACE CHARACTERISTICS OF SCOTS PINE WOOD HEATED AT HIGH TEMPERATURES AFTER WEATHERING
(Slovak Forest Products Research Inst, 2017)
This study was conducted to investigate some surface properties of wood specimens of heat treated Scots pine (Pinus sylvestris L.) after weathering such as surface hardness, surface roughness, gloss, and color changes. ...
SOME PHYSICAL CHARACTERISTICS OF THERMALLY MODIFIED ORIENTAL-BEECH WOOD
(Univ Bio-Bio, 2014)