A comparative study of magnetic, and magnetocaloric properties of different transition metal-doped La0.67Sr0.33AO3 (A: Mn, Co, Cr, and Fe) samples

Thumbnail

View/Open

Tam metin / Article (2.323Mb)

Date

2023

Author

Coşkun, A. Tulga
Ak, Y. Selim
Güleç N.
Akça, Gönül
Ekicibil A.
Coşkun, Atilla

Metadata

Show full item record

Citation

Coşkun, A.T., Ak, Y.S., Güleç, N. et al. A comparative study of magnetic, and magnetocaloric properties of different transition metal-doped La0.67Sr0.33AO3 (A: Mn, Co, Cr, and Fe) samples. J Mater Sci: Mater Electron 34, 1257 (2023). https://doi.org/10.1007/s10854-023-10654-w

Abstract

In the present work, structural, magnetic, and magnetocaloric properties of La0.67Sr0.33AO3 (A: Mn, Co, Cr and Fe) samples were examined. XRD analyses revealed that all samples produced by the sol–gel method and subjected to the same grinding and heat treatment steps crystallized in the perovskite crystal structure. In order to examine the magnetic behavior of the samples, temperature-dependent magnetization (M(T)) measurements were carried out. It was found that La0.67Sr0.33MnO3, which has the highest magnetization value, has the highest Curie temperature (T C = 368.2 K). In order to determine the magnetic phase transition order and calculate magnetic entropy change (- Δ SM) value, field-dependent magnetization (M(H)) measurements in the transition temperature region were carried at zero field-cooled (ZFC) and field-cooled (FC) processes. The maximum magnetic entropy change (-ΔSMmax) of La0.67Sr0.33MnO3 sample was calculated as 1.5 Jkg−1 K−1 under 1 T magnetic field change. La0.67Sr0.33CoO3 sample, in which antiferromagnetic (AFM) and ferromagnetic (FM) interactions coexist, exhibits a paramagnetic (PM)-FM phase transition at 244.1 K. At 1 T magnetic field change, the (-ΔSMmax) was found to be 0.145 Jkg−1 K−1 for this sample. La0.67Sr0.33CrO3 and La0.67Sr0.33FeO3 samples showed weak FM properties due to the different magnetic interactions originating from the ions in the B-sites of the samples. The magnetic phase transition is second-order for all samples.

Source

Journal of Materials Science: Materials in Electronics

Volume

34

Issue

16

URI

https://doi.org/10.1007/s10854-023-10654-w
https://hdl.handle.net/20.500.12809/10775

Collections

  • Fizik Bölümü Koleksiyonu [189]
  • Scopus İndeksli Yayınlar Koleksiyonu [6219]
  • WoS İndeksli Yayınlar Koleksiyonu [6466]



DSpace software copyright © 2002-2015  DuraSpace
Contact Us | Send Feedback
Theme by 
@mire NV
 

 




| Policy | Guide | Contact |

DSpace@Muğla

by OpenAIRE
Advanced Search

sherpa/romeo

Browse

All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsTypeLanguageDepartmentCategoryPublisherAccess TypeInstitution AuthorThis CollectionBy Issue DateAuthorsTitlesSubjectsTypeLanguageDepartmentCategoryPublisherAccess TypeInstitution Author

My Account

LoginRegister

DSpace software copyright © 2002-2015  DuraSpace
Contact Us | Send Feedback
Theme by 
@mire NV
 

 


|| Policy || Guide|| Instruction || Library || Muğla Sıtkı Koçman University || OAI-PMH ||

Muğla Sıtkı Koçman University, Muğla, Turkey
If you find any errors in content, please contact:

Creative Commons License
Muğla Sıtkı Koçman University Institutional Repository is licensed under a Creative Commons Attribution-NonCommercial-NoDerivs 4.0 Unported License..

DSpace@Muğla:


DSpace 6.2

tarafından İdeal DSpace hizmetleri çerçevesinde özelleştirilerek kurulmuştur.